SabikUltem MD137resin adalahAKA DU242HF, data awal, PEI + PCE, helm kebakaran, thermal imager.
| Mekanis | Nilai | Satuan | Standar |
| Tekanan tarik, yld, tipe I, 5 mm/menit | 75 | MPa | ASTM D 638 |
| Tekanan tarik, brk, tipe I, 5 mm/menit | 60 | % | ASTM D 638 |
| Tensile Modulus, 5 mm/min | 2410 | MPa | ASTM D 638 |
| Tekanan lentur, yld, 2,6 mm/menit, rentang 100 mm | 99 | MPa | ASTM D 790 |
| Flexural Modulus, 2,6 mm/menit, rentang 100 mm | 2340 | MPa | ASTM D 790 |
| Dampak | Nilai | Satuan | Standar |
| Izod Dampak, bertanduk, 23°C | 144 | J/m | ASTM D 256 |
| Termal | Nilai | Satuan | Standar |
| HDT, 1,82 MPa, 3,2 mm, tidak diiris | 160 | °C | ASTM D 648 |
| FISIK | Nilai | Satuan | Standar |
| Gravitasi Spesifik | 1.24 | - | ASTM D 792 |
| Tingkat Aliran Peleburan, 295°C/6,6 kgf | 35 | g/10 menit | ASTM D 1238 |
| Sumber GMD, terakhir diperbarui:09/01/2000 | |||
|
Untuk informasi lebih lanjut silahkan unduh lembar data |
|
| S-Plastics Ultem MD137.pdf | |
|
Dapatkan Kutipan Terbaru
Sumber distribusi tingkat pertama di Cina Selatan Mengurangi biaya pengadaan, meningkatkan stabilitas pasokan, Membantu Anda menemukan bahan plastik rekayasa yang paling cocok
|
![]()