SabikVertonR1000Iresin adalahKomposisi Nylon 66 High Impact yang mengandung Impact Modifier.
| Properti Tipikal (1) | |||
| Mekanis | Nilai | Satuan | Standar |
| Tekanan tegangan, istirahat | 45 | MPa | ISO 527 |
| Tekanan tarik, putus | 70 | % | ISO 527 |
| Modulus tarik, 1 mm/menit | 2200 | MPa | ISO 527 |
| Tekanan Flexural | 50 | MPa | ISO 178 |
| Modulus Flexural | 1400 | MPa | ISO 178 |
| Dampak | Nilai | Satuan | Standar |
| Izod Impact, tidak diukir 80*10*4 +23°C | 98 | kJ/m2 | ISO 180/1U |
| Izod Impact, bernotas 80*10*4 +23°C | 55 | kJ/m2 | ISO 180/1A |
| Termal | Nilai | Satuan | Standar |
| HDT/Af, 1,8 MPa Flatw 80*10*4 sp=64mm | 65 | °C | ISO 75/Af |
| FISIK | Nilai | Satuan | Standar |
| Penyusutan jamur, aliran, 24 jam | 1.1 - 1.5 | % | ISO 294 |
| Kepadatan | 1.09 | g/cm3 | ISO 1183 |
| Sumber GMD, terakhir diperbarui:09/30/2004 | |||
| Parameter | ||
| Pencetakan Injeksi | Nilai | Satuan |
| Suhu Pengeringan | 80 | °C |
| Waktu Pengeringan | 4 | jam |
| Kandungan Kelembaban Maksimal | 0.15 - 0.25 | % |
| Suhu Peleburan | 265 - 275 | °C |
| Suhu depan - Zona 3 | 260 - 270 | °C |
| Tengah - Zona 2 Suhu | 255 - 265 | °C |
| Bagian belakang - Zona 1 Suhu | 250 - 260 | °C |
| Suhu Cetakan | 60 - 100 | °C |
| Tekanan Belakang | 0.2 - 0.3 | MPa |
| Kecepatan sekrup | 30 - 60 | rpm |
| Sumber GMD, terakhir diperbarui:09/30/2004 | ||
Produk terkait lainnya yang kami rekomendasikan:
|
Untuk informasi lebih lanjut silahkan download lembar data |
|
| S-Plastics Verton R1000I.pdf | |
|
Dapatkan Kutipan Terbaru
Sumber distribusi tingkat pertama di Cina Selatan Mengurangi biaya pengadaan, meningkatkan stabilitas pasokan, Membantu Anda menemukan bahan plastik rekayasa yang paling cocok
|
![]()