SabikStat-konMX01739Cresin adalahsenyawa berbasis polipropilena yang mengandung Filler Proprietary. Karakteristik kelas ini adalah:
| Properti Tipikal (1) | |||
| Mekanis | Nilai | Satuan | Standar |
| Tekanan tarik, yld, tipe I, 5 mm/menit | 28 | MPa | ASTM D 638 |
| Tekanan tarik, yld, tipe I, 5 mm/menit | 0.8 | % | ASTM D 638 |
| Tensile Modulus, 50 mm/min | 6930 | MPa | ASTM D 638 |
| Tekanan lentur, yld, 1,3 mm/menit, rentang 50 mm | 41 | MPa | ASTM D 790 |
| Flexural Modulus, 1,3 mm/menit, rentang 50 mm | 5580 | MPa | ASTM D 790 |
| Tekanan tarik, hasil, 5 mm/menit | 25 | MPa | ISO 527 |
| Tekanan tarik, hasil, 5 mm/menit | 0.9 | % | ISO 527 |
| Modulus tarik, 1 mm/menit | 5240 | MPa | ISO 527 |
| Tekanan Flexural | 40 | MPa | ISO 178 |
| Flexural Modulus, 2 mm/menit | 5590 | MPa | ISO 178 |
| Dampak | Nilai | Satuan | Standar |
| Izod Dampak, tidak diukir, 23°C | 68 | J/m | ASTM D 4812 |
| Izod Dampak, bertanduk, 23°C | 34 | J/m | ASTM D 256 |
| Dampak Multiaxial | 4 | J | ISO 6603 |
| Energi Total Dampak Instrumen, 23°C | 15 | J | ASTM D 3763 |
| Izod Impact, tidak diukir 80*10*4 +23°C | 8 | kJ/m2 | ISO 180/1U |
| Izod Impact, bernotas 80*10*4 +23°C | 2 | kJ/m2 | ISO 180/1A |
| Termal | Nilai | Satuan | Standar |
| HDT, 0,45 MPa, 3,2 mm, tidak diiris | 134 | °C | ASTM D 648 |
| HDT, 1,82 MPa, 3,2 mm, tidak diiris | 94 | °C | ASTM D 648 |
| CTE, -30°C sampai 30°C, aliran | 1.7E+01 | 1/°C | ASTM D 696 |
| CTE, -30°C sampai 30°C, xflow | 7.74E+01 | 1/°C | ASTM D 696 |
| HDT/Bf, 0,45 MPa Flatw 80*10*4 sp=64mm | 125 | °C | ISO 75/Bf |
| HDT/Af, 1,8 MPa Flatw 80*10*4 sp=64mm | 83 | °C | ISO 75/Af |
| FISIK | Nilai | Satuan | Standar |
| Gravitasi Spesifik | 1.04 | - | ASTM D 792 |
| Kepadatan | 1.03 | g/cm3 | ASTM D 792 |
| Penyerapan Kelembaban, 50% RH, 24 jam | 0.02 | % | ASTM D 570 |
| Penyusutan jamur, aliran, 24 jam (5) | 0.6 - 0.9 | % | ASTM D 955 |
| Penyusutan jamur, xflow, 24 jam (5) | 1 - 4 | % | ASTM D 955 |
| Penyerapan Kelembaban (23°C / 50% RH) | 0.02 | % | ISO 62 |
| Listrik | Nilai | Satuan | Standar |
| Resistensi Permukaan | 4.E+00 - 7.E+00 | Ohm | ASTM D 257 |
| Sumber GMD, terakhir diperbarui:2009/09/02 | |||
| Parameter | ||
| Pencetakan Injeksi | Nilai | Satuan |
| Suhu Pengeringan | 80 | °C |
| Waktu Pengeringan | 4 | jam |
| Suhu Peleburan | 225 - 250 | °C |
| Suhu depan - Zona 3 | 240 - 250 | °C |
| Tengah - Zona 2 Suhu | 215 - 225 | °C |
| Bagian belakang - Zona 1 Suhu | 195 - 205 | °C |
| Suhu Cetakan | 30 - 50 | °C |
| Tekanan Belakang | 0.2 - 0.3 | MPa |
| Kecepatan sekrup | 30 - 60 | rpm |
| Sumber GMD, terakhir diperbarui:2009/09/02 | ||
Produk terkait lainnya yang kami rekomendasikan:
|
Untuk informasi lebih lanjut silahkan download lembar data |
|
| S-Plastics Stat-kon MX01739C.pdf | |
|
Dapatkan Kutipan Terbaru
Sumber distribusi tingkat pertama di Cina Selatan Mengurangi biaya pengadaan, meningkatkan stabilitas pasokan, Membantu Anda menemukan bahan plastik rekayasa yang paling cocok
|