S-Plastics LexanFL1600Pengurangan Berat Berbagai Pada 0,250 " (6,35 mm) Dinding.
Properti Tipikal (1) | |||
Mekanis | Nilai | Satuan | Standar |
busa - MEKANIS 6.4 mm Wt Pengurangan | 10 | % | - |
Tekanan tarik, hasil, 6,35 mm | 48 | MPa | ASTM D 638 |
Tekanan tarik, putus, 6,35 mm | 5.2 | % | ASTM D 638 |
Tensile Modulus, 6,4 mm | 2440 | MPa | ASTM D 638 |
Tekanan lentur, hasil, 6,4 mm | 89 | MPa | ASTM D 790 |
Flexural Modulus, 6,4 mm | 2750 | MPa | ASTM D 790 |
Dampak | Nilai | Satuan | Standar |
BUMEN - Dampak 6.4 mm Wt Pengurangan | 10 | % | - |
Izod Dampak, tidak diukir, 23°C | 747 | J/m | ASTM D 4812 |
Terjatuh Dart Dampak, 23°C | 56 | J | Metode S-Plastics |
Termal | Nilai | Satuan | Standar |
BUMEN - PEMERINTAH 6.4mm Wt Pengurangan | 10 | % | - |
HDT, 0,45 MPa, 6,4 mm, tidak diiris | 137 | °C | ASTM D 648 |
HDT, 1,82 MPa, 6,4 mm, tidak diiris | 126 | °C | ASTM D 648 |
CTE, -40°C sampai 95°C, aliran | 5.04E-05 | 1/°C | ASTM E 831 |
Panas spesifik | 1.15 | J/g-°C | ASTM C 351 |
FISIK | Nilai | Satuan | Standar |
busa - PHYSICAL 6.4mm Wt Pengurangan | 10 | % | - |
Gravitasi Spesifik | 1.25 | - | ASTM D 792 |
Gravitasi spesifik, cetakan busa | 1.13 | - | ASTM D 792 |
Penyerapan air, 24 jam | 0.14 | % | ASTM D 570 |
Penyerapan air, keseimbangan, 23C | 0.33 | % | ASTM D 570 |
Penyusutan jamur, aliran, 6,4 mm | 0.5 - 0.7 | % | Metode S-Plastics |
Listrik | Nilai | Satuan | Standar |
busa - Listrik 6.4 mm Wt Pengurangan | 20 | % | - |
Resistivitas Volume | 2.8E+17 | Ohm-cm | ASTM D 257 |
Resistensi Permukaan | >1.1E+17 | Ohm | ASTM D 257 |
Permittivitas relatif, 100 Hz | 2.45 | - | ASTM D 150 |
Permittivitas Relatif, 1 MHz | 2.44 | - | ASTM D 150 |
Faktor Dissipasi, 100 Hz | 0.007 | - | ASTM D 150 |
Faktor Dissipasi, 1 MHz | 0.0042 | - | ASTM D 150 |
Sumber GMD, terakhir diperbarui:08/07/1989 |
Parameter | ||
Membentuk busa struktural | Nilai | Satuan |
Agen Blowing, Sistem Fisik | Gas nitrogen | - |
Agen Blowing, Sistem Kimia | FLC298 | - |
Waktu Pengeringan (Agen Bertiup) | 4 | jam |
Suhu Pengeringan (Agen Bertiup) | 105 | °C |
Jangkauan konsentrasi (Agen Blowing) | 3 - 5 | % |
Konsentrasi yang Disarankan (Agen Blowing) | 1.5 | % |
Suhu pengeringan (resin) | 120 | °C |
Waktu pengeringan (resin) | 3 - 4 | jam |
Waktu pengeringan (resin, kumulatif) | 48 | jam |
Suhu Peleburan | 290 - 310 | °C |
Suhu Nozzle | 270 - 295 | °C |
Suhu Depan | 290 - 305 | °C |
Suhu Rata-rata | 290 - 305 | °C |
Suhu Belakang | 255 - 280 | °C |
Suhu Cetakan | 70 - 95 | °C |
Sumber GMD, terakhir diperbarui:08/07/1989 |
Untuk informasi lebih lanjut silahkan download lembar data |
|
![]() |